News
-
Media center
-
Hose knowledge
*
any characters
?
single character
Electrical properties
General information
When solids and liquids are conveyed through hoses, friction between the conveyed material and the hose wall can generate an electrostatic charge. To determine the electrical properties of a hose — and therefore its tendency to accumulate electrostatic charge — Norres Baggerman tests the conductivity of hoses in accordance with the requirements of DIN EN ISO 8031.
To measure the electrical properties in accordance with DIN EN ISO 8031, the hose is placed on a non-conductive surface.
As a general rule, Norres Baggerman tests every batch for conductivity and electrical properties. The measured values are archived in a traceable manner. Customers may obtain a corresponding test certificate for the batches they have purchased.
Measurement of Surface resistance
Conductive sponges are used to determine the surface resistance of the hose. The sponges are connected to the measuring instrument using crocodile clips and attached to both sides of the hose. To reduce contact resistance, the sponges should be in full contact with the hose surface.
Measurement of resistance through the hose wall
When measuring resistance through the hose wall, one of the conductive sponges is removed and the crocodile clip is attached to the wire or stranded conductor of the hose instead. This measures the resistance between the inner hose wall and the conductor.
Measurement in accordance with TRGS
The Norres Baggerman Group, in collaboration with external experts, has determined which hoses are suitable for use in potentially explosive atmospheres in accordance with TRGS 727 for each hose type.
The measurement method used for this purpose is described in DIN EN ISO 8031 and is based on the measurement of resistance through the hose wall described above. The difference is that the sponge and wire are positioned on the same side. The measured resistance is then converted into the specific resistance required by TRGS 727.
Other measurement methods
Depending on the product being tested, the measurements can be adapted to its specific characteristics. For example, no sponge soaked in conductive fluid is used for highly conductive cuffs or hoses from the Norres Baggerman product range. Instead, a specially formulated conductive silver coating or a metallic test core is used to minimise the contact resistance between the electrode and the clip.
Measuring instruments
- Resistance values > 1.0 × 10⁶ Ω are measured at a test voltage of 500 V (Metriso Tech).
- Resistance values < 1.0 × 10⁶ Ω are measured at a test voltage of 40 V (Voltcraft multimeter).
Do you have any questions about electrical property measurements?
The Norres Baggerman Group’s team of experts will be happy to assist you!
Subject to technical modifications.